Kas Inconel 600 saab keevitada?
Inconel-Keemiline koostis
Inconel | Ni | Kr | Fe | Mo | Nb | Kaas | Mn | Cu | Al | Ti | Si | C | S | P | B |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
600 | 72 | 14.0-17.0 | 6.0-10.0 | 1 | 0.5 | 0.5 | 0.15 | 0.015 | |||||||
617 | 44.2-56.0 | 20.0-24.0 | 3 | 8.0-10.0 | 10.0-15.0 | 0.5 | 0.5 | 0.8-1.5 | 0.6 | 0.5 | 0.15 | 0.015 | 0.015 | 0.006 | |
625 | 58 | 20.0-23.0 | 5 | 8.0-10.0 | 3.15-4.15 | 1 | 0.5 | 0.4 | 0.4 | 0.5 | 0.1 | 0.015 | 0.015 | ||
690 | 59.5 | 30 | 9.2 | 0.35 | 0.01 | 0.02 | 0.35 | 0.019 | 0.003 | ||||||
718 | 50.0-55.0 | 17.0-21.0 | tasakaalu | 2.8-3.3 | 4.75-5.5 | 1 | 0.35 | 0.2-0.8 | 0.65-1.15 | 0.3 | 0.35 | 0.08 | 0.015 | 0.015 | 0.006 |
X-750 | 70 | 14.0-17.0 | 5.0-9.0 | 0.7-1.2 | 1 | 1 | 0.5 | 0.4-1.0 | 2.25-2.75 | 0.5 | 0.08 | 0.01 |
Inconel 600 keevitusomadused
Inconel 600 keevitamine ei vaja üldjuhul eelsoojendust. Kui aga mitteväärismetalli temperatuur on madalam kui 15 kraadi, tuleks mõlemalt poolt 250–300 mm pikkust liitekohta eelsoojendada temperatuurini 15–20 kraadi, et vältida niiskuse kondenseerumisest tingitud pooride tekkimist. Terade kasvu ja karbiidisademete vältimiseks ei tohiks vooludevaheline temperatuur olla kõrgem kui 100 kraadi. Ettevaatlik tuleb olla, et vältida kiiret jahtumist, mis võib põhjustada poorsust. Enne keevitamist tuleb keevitusala hoolikalt puhastada.